物品名称 规格型号 数量 单位 描述
| 石墨环 |
ф228(进口)/243.96*233. |
100.00 |
个 |
{"规格":"ф228(进口)/243.96*233.96*34.8","抗压强度":">90Mpa","热膨胀系数":"3.2*10-6m/k","电阻率":"1210-6Ωm","洛氏硬度":"80","抗折强度":">49Mpa","渗透系数":"8-10cm2/s","体积密度":"1.72g/cm3","外形尺寸":"ф243.96mm*233.96mm*34.8mm","材质":"石墨","使用寿命":"400铸次天","参照标准":"GB/T 24528-2009","备注":"要求:进口石墨原料,石墨环上沿、石墨环底部位置必须涂刷密封漆,防止油气泄漏。\n设备厂家:美国瓦格斯塔夫\n设备名称:铸造盘\n设备型号:Φ228\n石墨环表面要光洁,无划痕,无凹坑,无裂纹、透油透气均匀\n石墨环性能达不到要求,厂家30天内无偿退换货"} |
| 石墨环 |
ф410*15/433.8*421.8* |
15.00 |
个 |
{"规格":"ф410*15/433.8*421.8*29.6","抗压强度":">90Mpa","热膨胀系数":"3.2*10-6m/k","电阻率":"1210-6Ωm","洛氏硬度":"80","抗折强度":">45Mpa","渗透系数":"0.25cm2/s","体积密度":"1.72g/cm3","外形尺寸":"ф433.8mm*421.8mm*29.6mm","材质":"石墨","使用寿命":"正常使用:30(≥200铸次)天","参照标准":"GB/T 24528-2009","备注":"1、要求:进口石墨原料,石墨环顶端、石墨环底部位置必须涂刷密封漆,防止油泄漏。\n2、设备信息:国产\n3、设备厂家:******公司\n4、设备名称:铸造盘、\n5、设备型号:Φ410*15\n6、异议处理:石墨环表面要光洁,无划痕,无凹坑,无裂纹、透油透气均匀、石墨环上下沿必须涂刷密封漆,石墨环性能达不到要求,厂家30天内无偿退换货,所产生的费用由厂家自行承担"} |
| 石墨环 |
ф152*72/166.5*156.6* |
150.00 |
个 |
{"规格":"ф152*72/166.5*156.6*26.8","抗压强度":">90Mpa","热膨胀系数":"3.2*10-6m/k","电阻率":"1210-6Ωm","洛氏硬度":"80","抗折强度":">45Mpa","渗透系数":"0.25cm2/s","体积密度":"1.72g/cm3","外形尺寸":"ф166.5mm*156.6mm*26.8mm","材质":"石墨","使用寿命":"正常使用:30(≥200铸次)天","参照标准":"GB/T 24528-2009","备注":"1、要求:进口石墨原料,石墨环上沿、石墨环底部位置必须涂刷密封漆,防止油气泄漏。\n2、设备信息:国产\n3、设备厂家:******公司\n4、设备名称:铸造盘、\n5、设备型号:Φ152*72\n6、石墨环到货时要提供原材料报关单及合格证\n7、异议处理:石墨环表面要光洁,无划痕,无凹坑,无裂纹、透油透气均匀、石墨环上下沿必须涂刷密封漆,石墨环性能达不到要求,厂家30天内无偿退换货,所产生的费用由厂家自行承担"} |
| 石墨环 |
ф88*112/100mm*89.7mm |
200.00 |
个 |
{"规格":"ф88*112/100mm*89.7mm*16mm","抗压强度":">90Mpa","热膨胀系数":"3.2*10-6m/k","电阻率":"1210-6Ωm","洛氏硬度":"80","抗折强度":">40Mpa","渗透系数":"0.25cm2/s","体积密度":"1.72g/cm3","外形尺寸":"ф100mm*89.7mm*16mm","材质":"石墨","使用寿命":"正常使用:30(≥200铸次)天","参照标准":"GB/T 24528-2009","备注":"1、要求:进口石墨原料\n2、设备信息:国产\n3、设备厂家:******公司\n4、设备名称:铸造盘、\n5、设备型号:Φ88*112\n6、异议处理:石墨环表面要光洁,无划痕,无凹坑,无裂纹、石墨环性能达不到要求,厂家30天内无偿退换货,所产生的费用由厂家自行承担"} |
| 石墨环 |
ф128*54/140*129.7**2 |
60.00 |
个 |
{"规格":"ф128*54/140*129.7**26.4","抗压强度":">90Mpa","热膨胀系数":"2.9m/k","电阻率":"1210-6Ωm","洛氏硬度":"80","抗折强度":">40Mpa","渗透系数":"0.25cm2/s","体积密度":"1.72g/cm3","外形尺寸":"ф140mm*129.7mm*26.4mm","材质":"石墨","使用寿命":"250铸次(30天)天","参照标准":"GB/T 24528-2009","备注":"要求:进口石墨原料,石墨环表面要光洁、无划痕、无凹坑、无裂纹\n设备厂家:****、\n设备名称:铸造盘、\n设备型号:Φ127*54\n异议处理:石墨环性能达不到要求,厂家30天内无偿退换货,所产生的费用由厂家自行承担"} |
| 石墨环 |
ф152*40/166.5*156.5* |
60.00 |
个 |
{"规格":"ф152*40/166.5*156.5*27.2","抗压强度":">90Mpa","热膨胀系数":"2.9m/k","电阻率":"1210-6Ωm","洛氏硬度":"80","抗折强度":">40Mpa","渗透系数":"0.25cm2/s","体积密度":"1.72g/cm3","外形尺寸":"ф166.5mm*156.5mm*27.2mm","材质":"石墨","使用寿命":"250铸次(30天)天","参照标准":"GB/T 24528-2009","备注":"要求:进口石墨原料,石墨环要光洁,无划痕,无凹坑,无裂纹,石墨环上下沿必须涂刷密封漆,防止油气泄漏。\n生产厂家: ****\n设备名称: 铸造盘\n设备型号:Φ152*40\n异议处理:石墨环性能达不到要求,厂家30天内无偿退换货,所产生的费用由厂家自行承担"} |
| 石墨环 |
ф330*15/350.7*339.6* |
40.00 |
个 |
{"规格":"ф330*15/350.7*339.6*20.64","抗压强度":">90Mpa","热膨胀系数":"2.9m/k","电阻率":"1210-6Ωm","洛氏硬度":"80","抗折强度":">40Mpa","渗透系数":"0.25cm2/s","体积密度":"1.72g/cm3","外形尺寸":"ф350.7mm*339.6mm*20.64mm","材质":"石墨","使用寿命":"250铸次天","参照标准":"GB/T 24528-2009","备注":"要求:进口石墨原料,石墨环表面要光洁、无划痕、无凹坑、无裂纹,石墨环上下沿必须涂刷密封漆,防止油气泄漏\n设备厂家:****、\n设备名称:铸造盘、\n设备型号:Φ330*15\n异议处理:石墨环性能达不到要求,厂家30天内无偿退换货,所产生的费用由厂家自行承担"} |
| 石墨环 |
ф300*32 |
50.00 |
个 |
{"规格":"ф300*32","抗压强度":">90Mpa","热膨胀系数":"2.9m/k","电阻率":"1210-6Ωm","洛氏硬度":"80","抗折强度":">40Mpa","渗透系数":"0.25cm2/s","体积密度":"1.72g/cm3","外形尺寸":"ф318mm*307.7mm*38.4mm","材质":"石墨","使用寿命":"250铸次(30天)天","参照标准":"GB/T 24528-2009","备注":"要求:进口石墨原料,石墨环上沿、石墨环底部位置必须涂刷密封漆,防止油气泄漏,石墨环表面要光洁,无划痕,无凹坑,无裂纹、透油透气均匀,设备厂家:美国瓦格斯塔夫,设备名称:铸造盘,设备型号:Φ300*32,异议处理:石墨环性能达不到要求,厂家30天内无偿退换货,所产生的费用由厂家自行承担"} |